Stacking
On dry and surface to avoid damage

 

Mortar For Masonry
AAC Mortar Mix or cement: sand (1:6)

 

Wetting of Block
Before Application Dip in water & lift immediately

 

Mortar Thickness
Keep it Limited to 10 to 12mm

             

Curing of Masonry Wall
Curing required only for mortar joint

 

Cutting of Block
Use tool like Hacksaw or hammer.

 

Electric & Sanitary Chasis
To be grooved before Plaster of wall

 

Plaster
Minimum external plaster thickness